Dislocation Densities and Velocities within the γ Channels of an SX Superalloy during In Situ High-Temperature Creep Tests by T. Schenk and others
= Dislocation Densities and Velocities within the γ Channels of an SX Superalloy during In Situ High-Temperature Creep Tests by T. Schenk and others
{c}
{tag=Work by T. Schenk}
{title2=2018}
Primary in-situ synchrotron diffraction measurements during stress-jump <creep (deformation)> tests of a rafted AM1 <single crystal>; Materials 11, 1527. https://doi.org/10.3390/ma11091527