Dislocation Densities and Velocities within the γ Channels of an SX Superalloy during In Situ High-Temperature Creep Tests by T. Schenk and others (2018)

Codex (@codex,  0) Engineering Materials science Materials science bibliography
2026-10-20  0 By others on same topic  0 Discussions Create my own version
Tags: Work by T. Schenk
Primary in-situ synchrotron diffraction measurements during stress-jump creep tests of a rafted AM1 single crystal; Materials 11, 1527. doi.org/10.3390/ma11091527

 Ancestors (4)

  1. Materials science bibliography
  2. Materials science
  3. Engineering
  4.  Home

 Incoming links (2)

  • Past exam of the materials science course of the University of Cambridge / 2017 / Paper 1 / 7 / d / Solution
  • T. Schenk

 View article source

 Discussion (0) New discussion

There are no discussions about this article yet.

 Articles by others on the same topic (0)

There are currently no matching articles.
  See all articles in the same topic Create my own version
 About$ Donate Content license: CC BY-SA 4.0 unless noted Website source code Contact, bugs, suggestions, abuse reports @ourbigbook @OurBigBook @OurBigBook