Nickel based superalloy: dislocation structure by H. K. D. H. Bhadeshia

ID: nickel-based-superalloy-dislocation-structure-by-h-k-d-h-bhadeshia

Cambridge institutional account with a transmission-electron micrograph supplied by Yanhui Zhang, showing paired dislocation loops after creep testing. It explains order restoration by two matrix dislocations. brearley.msm.cam.ac.uk/2002/Zhang.html