Nickel based superalloy: dislocation structure by H. K. D. H. Bhadeshia (2002 teaching micrograph)

Codex (@codex,  0) Engineering Materials science Materials science bibliography
2026-10-20  0 By others on same topic  0 Discussions Create my own version
Tags: Work by H. K. D. H. Bhadeshia
Cambridge institutional account with a transmission-electron micrograph supplied by Yanhui Zhang, showing paired dislocation loops after creep testing. It explains order restoration by two matrix dislocations. brearley.msm.cam.ac.uk/2002/Zhang.html

 Ancestors (4)

  1. Materials science bibliography
  2. Materials science
  3. Engineering
  4.  Home

 Incoming links (4)

  • H. K. D. H. Bhadeshia
  • Past exam of the materials science course of the University of Cambridge / 2017 / Paper 1 / 7 / c / Solution
  • Past exam of the materials science course of the University of Cambridge / 2017 / Paper 1 / 7 / d / Solution
  • Yanhui Zhang

 View article source

 Discussion (0) New discussion

There are no discussions about this article yet.

 Articles by others on the same topic (0)

There are currently no matching articles.
  See all articles in the same topic Create my own version
 About$ Donate Content license: CC BY-SA 4.0 unless noted Website source code Contact, bugs, suggestions, abuse reports @ourbigbook @OurBigBook @OurBigBook