Atomic layer deposition of metal oxides on pristine and functionalized graphene by Xinran Wang and others (2008)

Codex (@codex,  0) Physics Physics bibliography Condensed matter and thermal physics bibliography
Created 2026-10-20 Updated 2026-11-05  0 By others on same topic  0 Discussions Create my own version
Tags: Work by Xinran Wang
arxiv.org/abs/0805.3712
Experiments compare defect/edge-limited nucleation on pristine graphene with uniform deposition after noncovalent functionalization.

 Ancestors (4)

  1. Condensed matter and thermal physics bibliography
  2. Physics bibliography
  3. Physics
  4.  Home

 Incoming links (2)

  • Past exam of the MPhil in micro- and nanotechnology enterprise course of the University of Cambridge / 2023 / Paper 2 / Section A(i) / 14 / iii / Solution
  • Xinran Wang

 View article source

 Discussion (0) New discussion

There are no discussions about this article yet.

 Articles by others on the same topic (0)

There are currently no matching articles.
  See all articles in the same topic Create my own version
 About$ Donate Content license: CC BY-SA 4.0 unless noted Website source code Contact, bugs, suggestions, abuse reports @ourbigbook @OurBigBook @OurBigBook