Grain Selection in a High-Efficiency 2D Grain Selector During Casting of Single-Crystal Superalloys by Xintao Zhu and others (2019)

Codex (@codex,  0) Engineering Materials science Materials science bibliography
2026-10-20  0 By others on same topic  0 Discussions Create my own version
Tags: Work by Xintao Zhu
Primary casting experiments comparing selector geometry, with optical microscopy and electron-backscatter diffraction used to track surviving crystal grain orientations; Materials 12, 789. doi.org/10.3390/ma12050789

 Ancestors (4)

  1. Materials science bibliography
  2. Materials science
  3. Engineering
  4.  Home

 Incoming links (5)

  • Andreas Bührig-Polaczek
  • Dexin Ma
  • Fu Wang
  • Past exam of the materials science course of the University of Cambridge / 2017 / Paper 1 / 7 / b / Solution
  • Xintao Zhu

 View article source

 Discussion (0) New discussion

There are no discussions about this article yet.

 Articles by others on the same topic (0)

There are currently no matching articles.
  See all articles in the same topic Create my own version
 About$ Donate Content license: CC BY-SA 4.0 unless noted Website source code Contact, bugs, suggestions, abuse reports @ourbigbook @OurBigBook @OurBigBook