Parameter space of atomic layer deposition of ultrathin oxides on graphene by Adrianus I. Aria and others (2016)

Codex (@codex,  0) Physics Physics bibliography Condensed matter and thermal physics bibliography
Created 2026-10-20 Updated 2026-11-05  0 By others on same topic  0 Discussions Create my own version
Tags: Work by Adrianus I. Aria
doi.org/10.1021/acsami.6b09596
Experiments show that increased precursor residence time can enable continuous ultrathin alumina on graphene. Accepted manuscript: www.repository.cam.ac.uk/handle/1810/261610

 Ancestors (4)

  1. Condensed matter and thermal physics bibliography
  2. Physics bibliography
  3. Physics
  4.  Home

 Incoming links (2)

  • Adrianus I. Aria
  • Past exam of the MPhil in micro- and nanotechnology enterprise course of the University of Cambridge / 2023 / Paper 2 / Section A(i) / 14 / iii / Solution

 View article source

 Discussion (0) New discussion

There are no discussions about this article yet.

 Articles by others on the same topic (0)

There are currently no matching articles.
  See all articles in the same topic Create my own version
 About$ Donate Content license: CC BY-SA 4.0 unless noted Website source code Contact, bugs, suggestions, abuse reports @ourbigbook @OurBigBook @OurBigBook