Primary recommendation: doi.org/10.1351/PAC-REC-10-12-04 . Pure and Applied Chemistry 84(2), 377–410 (2012). Verified publisher byline: Michel Vert, Yoshiharu Doi, Karl-Heinz Hellwich, Michael Hess, Philip Hodge, Przemyslaw Kubisa, Marguerite Rinaudo and François Schué. Official PDF: publications.iupac.org/pac/pdf/2012/pdf/8402x0377.pdf . Entries 30 (biomaterial) and 106 (biocompatibility in biomedical therapy). Entry 30 is reproduced in the primary IUPAC Gold Book goldbook.iupac.org/terms/view/13881 .
Additional precise locator: entry 70, erosion, printed p. 391, defines degradation beginning at the surface and progressing inward; its notes discuss reaction versus reagent diffusion and discourage the wording bulk erosion. The official Gold Book reproduces this definition at goldbook.iupac.org/terms/view/13906 . Both the indexed primary recommendation and Gold Book entry were verified; direct-reader access to the PDF/entry returned 403. A mass-loss curve alone does not establish the spatial mechanism.
Ancestors (4)
Incoming links (9)
Discussion (0) New discussion
There are no discussions about this article yet.
Articles by others on the same topic (0)
There are currently no matching articles.