An alloy developed to sustain mechanical load at high temperatures while resisting creep and environmental attack.
A high-temperature alloy based on a nickel-rich disordered matrix, commonly strengthened by ordered precipitates and substitutional solutes.
A turbine blade cast as one crystal to remove high-temperature grain boundary sliding and grain-boundary cavitation pathways. This does not eliminate dislocations or all sources of creep.
The ordered phase based on in many nickel-based superalloys. A matrix translation disrupts its order and can create an antiphase boundary.
Articles by others on the same topic
Superalloys, also known as high-performance alloys, are a class of materials that are designed to withstand extreme conditions, such as high temperatures, high mechanical stress, and corrosive environments. These alloys are primarily used in applications where durability and reliability are crucial, such as in the aerospace, power generation, and automotive industries.